Henan Bellian Mining Machinery
Home/ Solutions/ Mineral Processing/ Process route
Mineral Processing · Process route

Gold Ore Flotation Line

Reviewed 2026-11-27 Bellian Process Engineering

Flotation route for gold locked in sulphides: bulk or selective flotation of pyrite and arsenopyrite, 85-92% recovery into a concentrate of 20-60 g/t for smelting or roasting.

Gold Ore Flotation Line

If a bottle roll test recovers less than 85% of the gold, the gold is locked in sulphides and cyanide alone will not reach it. The answer is usually flotation: concentrate the sulphide carrying the gold into 3-10% of the mass, then either sell that concentrate or treat it further. Flotation does not dissolve the gold, it just makes the problem small enough to handle.

Capacity100-1,000 t/d
Concentrate20-60 g/t Au
Mass pull3-10%
Recovery85-92%

Bulk or selective

Bulk flotation floats all the sulphides together and maximises gold recovery at the cost of a low-grade concentrate. Selective flotation floats pyrite and arsenopyrite separately, giving a cleaner concentrate that smelters pay more for, at 3-5% lower recovery. The choice is commercial: if there is a smelter within reach, selective is better; if the concentrate has to be shipped 5,000 km, bulk with a higher grade usually wins.

Process flow

CrushingGrindingRougher flotationScavengerCleaner (2 stages)ThickeningFiltration

Grind size is the whole game

Gold-bearing sulphides typically need 60-80% passing 75 microns to liberate. Over-grinding produces slimes that report to tails and are lost; under-grinding leaves locked particles that float but do not smelt well. A Ball Mill with a hydrocyclone and a variable-speed drive lets the operator find the right point, which is usually narrower than the textbook suggests.

Flotation circuit

Rougher at pH 8.5-9.5 with potassium amyl xanthate at 60-120 g/t and MIBC frother. Scavenger on the rougher tail with additional collector. Two cleaner stages produce the final concentrate. Where arsenopyrite is present, pH is raised to 11 with lime to depress it and float pyrite selectively.

StageReagentDosePurpose
GrindingLime1-3 kg/tpH control, pyrite depression at high pH
RougherPotassium amyl xanthate60-120 g/tSulphide collector
RougherMIBC20-40 g/tFrother
CleanerSodium cyanide50-150 g/tDepress pyrite, float arsenopyrite

What happens to the concentrate

Three options, decided by grade and by what is locally available. Direct smelting works above 40 g/t with low arsenic. Roasting or bio-oxidation before cyanidation unlocks arsenopyrite-hosted gold at 90-95% recovery. Pressure oxidation does the same faster but needs 20-40 bar autoclaves and is only economic above 1,000 t/d of concentrate.

Questions we are asked before quoting

Why not just cyanide the whole ore?

Because locked gold does not dissolve. If the bottle roll gives 60%, cyanidation loses 40% of your gold no matter how much cyanide you add. Flotation first is the only fix.

What grade of concentrate do I need?

Above 20 g/t Au to be saleable, above 40 g/t to smelt directly. Below 20 g/t the transport cost usually exceeds the contained value unless the smelter is very close.

Other solution categories

Same engineering team, different process route.

Send your material. We will send the flow sheet.

Feed size, moisture, target capacity and product spec are enough to start. Quotations and plant layouts are free and usually back within one working day.

Request a flow sheet WhatsApp us