Henan Bellian Mining Machinery
Home/ Solutions/ Mineral Processing/ Process route
Mineral Processing · Process route

Lithium Spodumene Beneficiation Line

Reviewed 2026-11-27 Bellian Process Engineering

Spodumene concentration by dense media pre-concentration and flotation, producing 5.5-6.0% Li2O concentrate at 75-85% recovery for the battery supply chain.

Lithium Spodumene Beneficiation Line

Spodumene is a hard, coarse-grained mineral that responds well to dense media separation — which is unusual among lithium minerals and is the reason spodumene dominates hard-rock lithium supply. The design question is how much to pre-concentrate before flotation, because DMS is cheap per tonne and flotation is not.

Capacity300-2,000 t/d
Feed grade1.0-1.8% Li2O
Concentrate5.5-6.0% Li2O
Recovery75-85%

Why dense media first

Spodumene has a specific gravity of 3.1-3.2, against 2.6 for quartz and feldspar. A dense media cyclone at 2.7-2.8 SG rejects 30-50% of the feed as barren light material at a cost of about USD 1.20 per tonne. Doing that before flotation removes the same proportion of the flotation reagent bill and the flotation plant capacity.

The limit is liberation. DMS only works above about 0.5 mm, so if the spodumene is finely disseminated the rejection rate falls and the economics deteriorate.

Process flow

CrushingScreening 0.5-10 mmDense media cycloneGrindingDeslimingFlotationMagnetic removalFiltration

Crushing and DMS

Two-stage crushing to 10 mm, then screening at 0.5 mm. The 0.5-10 mm fraction goes to a dense media cyclone at 2.7 SG; floats go to tailings, sinks go to grinding. The minus 0.5 mm fraction bypasses DMS and goes straight to flotation, which is where 15-25% of the lithium sits.

Grinding and desliming

A Ball Mill to 80% passing 150 microns. Desliming at 20 microns in a cyclone is critical: slimes consume collector and depress flotation, and spodumene plants that skip this stage run 10 points lower on recovery.

Flotation

Two routes. Fatty acid flotation at pH 8-9 with sodium silicate depressant works on clean ore and is cheap. Cationic flotation with an amine collector at pH 3-4 after sulphuric acid conditioning is more selective and handles ore with mica. Most modern plants use the second, despite the acid handling.

Equipment list

StageEquipmentNote
CrushingJaw + cone to 10 mmTwo stage, minimise fines
DMSDense media cyclone 500 mm + ferrosilicon circuit2.7 SG cut
GrindingBall mill 2,400 x 4,50080% passing 150 micron
DeslimingCyclone cluster at 20 micronCritical for recovery
FlotationRougher 6 + cleaner 3 + scavenger 4Amine or fatty acid
MagneticWet high-intensity, 1.2 TRemove iron-bearing garnet
DewateringThickener + pressure filter8% moisture for shipping

The iron penalty

Spodumene concentrate is sold on Li2O but penalised on Fe2O3. Above 1.2% Fe2O3 the concentrate is discounted because iron reports to the leach and complicates the conversion route. The usual source is garnet and biotite, both removed by a wet high-intensity magnetic pass after flotation. This is not optional for battery-grade concentrate.

Questions we are asked before quoting

Can I produce battery-grade lithium carbonate directly?

No. Beneficiation produces a 5.5-6% Li2O concentrate; conversion to carbonate needs a roasting and hydrometallurgical plant, which is a separate project at 10-20 times the capital.

How much water does the plant need?

2.5-4 m3 per tonne of ore in a closed circuit. Lithium plants in Western Australia operate on bore water with a thickener and return water dam.

Other solution categories

Same engineering team, different process route.

Send your material. We will send the flow sheet.

Feed size, moisture, target capacity and product spec are enough to start. Quotations and plant layouts are free and usually back within one working day.

Request a flow sheet WhatsApp us