Henan Bellian Mining Machinery
Home/ Solutions/ Powder Grinding/ Process route
Powder Grinding · Process route

Quicklime and Hydrated Lime Powder Line

Reviewed 2026-11-27 Bellian Process Engineering

From limestone to bagged lime: calcination at 900-1100 C, slaking and classification, producing quicklime at 85-92% CaO or hydrated lime at 92-96% Ca(OH)2.

Quicklime and Hydrated Lime Powder Line

Lime is a two-stage product and most plants only get one stage right. Calcination produces quicklime; slaking and classification produce hydrated lime. A plant that has a good kiln but a rough slaker ends up selling quicklime at commodity prices while its hydrated lime goes to the low-value markets. The slaker is where the margin is made.

Capacity50-500 t/d
Quicklime85-92% CaO
Hydrated92-96% Ca(OH)2
Kiln temp900-1100 C

Calcination: the kiln decision

Three kiln types serve different scales. A vertical shaft kiln is the most efficient per tonne for small and medium output but needs lump limestone in a narrow size band (40-80 mm). A rotary kiln accepts a wider feed size but loses heat and needs more fuel. A preheater rotary kiln sits between them.

Kiln typeCapacityFuelFeed size
Vertical shaft50-300 t/d70-90 kg coal/t40-80 mm, uniform
Preheater rotary200-600 t/d95-115 kg coal/t10-40 mm
Long rotary150-500 t/d120-150 kg coal/t0-30 mm

Process flow

Quarry limestoneCrushing and screeningKilnCoolerQuicklime storageSlakerClassifierHydrated lime

Feed preparation

Size consistency decides kiln performance more than anything else. A shaft kiln fed with a 40-80 mm band runs at 88-92% CaO; the same kiln fed 20-100 mm runs at 75-82% because the fines over-burn and the lumps under-burn. Screening before the kiln is not optional.

Calcination

A rotary kiln at 900-1,100 C with 2.5-3.5 hours residence. The dissociation of CaCO3 needs 1,780 kJ per kg, which sets the theoretical fuel floor at about 75 kg of coal per tonne of lime; anything above 110 kg means heat is being lost through the shell or the exhaust.

Slaking

Quicklime plus water gives Ca(OH)2 and releases a lot of heat. The slaker has to add water at a controlled rate, keep the mixture moving, and remove grit. A two-stage slaker with a classifier produces 92-96% Ca(OH)2 with less than 1% residue on a 45 micron screen. Insufficient water gives a dry, dusty product with unreacted cores; excess water gives a slurry that has to be dried at great cost.

Equipment list

StageEquipmentSpecification
CrushingJaw crusher + vibrating screen40-80 mm kiln feed
KilnRotary kiln 2.5 x 50 m200 t/d, 1,050 C
CoolerRotary coolerTo 80 C
SlakerTwo-stage, 15 t/hWater ratio controlled
ClassifierAir classifier325 mesh, less than 1% residue
CollectionBag filter20 mg/m3
PackingValve packer 50 kg + bulk loadingBoth formats

Quality control that customers actually check

Available lime (ASTM C25 or the sucrose method), residue on 45 and 75 micron, bulk density, and CO2 content for under-burnt stone. A hydrated lime at 93% Ca(OH)2 with 2% residue sells at a discount to one at 95% with 0.5% residue, and the difference is entirely in the slaker and classifier settings.

Questions we are asked before quoting

Can I make both quicklime and hydrated lime?

Yes, and that is the usual arrangement. Quicklime is sold in lumps or ground, hydrated lime is sold bagged. The slaker needs only about 25% of the capital of the kiln line.

What limestone quality do I need?

Above 93% CaCO3 for building lime, above 96% for chemical use. Silica and alumina above 3% cause ring formation in the kiln and reduce the reactivity of the product.

Other solution categories

Same engineering team, different process route.

Send your material. We will send the flow sheet.

Feed size, moisture, target capacity and product spec are enough to start. Quotations and plant layouts are free and usually back within one working day.

Request a flow sheet WhatsApp us