Magnetite Beneficiation Line

Reviewed 2026-11-27 Bellian Process Engineering

Magnetite concentration by staged grinding and low-intensity magnetic separation, reaching 65-68% Fe at 85-92% recovery with a 3-stage cobber-rougher-cleaner circuit.

Magnetite Beneficiation Line

Magnetite is the easiest iron mineral to concentrate and the easiest to over-grind. It responds to a magnetic field at 1,200-1,600 gauss, which means you can reject a large part of the gangue early and cheaply — but only if the crushing circuit has liberated the magnetite without crushing it to slime. The whole design of a magnetite plant is about removing barren rock as early as possible.

Capacity300-3,000 t/d
Feed grade25-40% Fe
Concentrate65-68% Fe
Recovery85-92%

Staged grinding, staged separation

A single grind to 75 microns and one magnetic pass will give you a 62% concentrate. Three stages of grinding with a magnetic separation after each will give 67% at higher recovery, for maybe 20% more grinding power. The difference is that each stage rejects gangue before it is ground further, so you stop paying to grind waste.

CircuitGrindConcentrateRecovery
Single stage75 micron62-64% Fe88%
Two stage75 + 45 micron65-66% Fe90%
Three stage75 + 45 + 25 micron67-68% Fe92%

Process flow

Crushing to 10 mmCobber (dry or wet)Stage 1 grindingRougher LIMSStage 2 grindingCleaner LIMSFiltration

Crushing and cobbing

A jaw crusher followed by a cone crusher to 10 mm. A dry cobber magnetic pulley on the conveyor ahead of the mill rejects 15-25% of the feed as barren rock at almost no operating cost. This is the cheapest tonnage you will ever remove.

Grinding and separation

Stage 1 is a Ball Mill to 75 microns followed by a wet low-intensity drum separator at 1,200 gauss. The rougher concentrate is reground to 45 microns and cleaned at 1,500 gauss. A third stage to 25 microns is only worth it if the magnetite is finely disseminated, which a liberation study will tell you before you spend the money.

Dewatering

Magnetic concentrate dewarers fast. A 12 m thickener plus a disc filter gives 9-10% moisture, which is what a pellet plant or a sinter plant wants. Higher moisture means paying to ship water.

Equipment list

StageEquipmentSpecification
PrimaryPE-750x1060 jawTo 100 mm
SecondaryHPT300 coneTo 10 mm
CobbingDry magnetic pulley, 1,200 gaussReject 15-25%
Stage 1Ball mill 2,400 x 4,50075 micron
RougherCTB-1230 wet drum, 1,200 gaussRougher concentrate
Stage 2Ball mill 1,800 x 4,00045 micron
CleanerCTB-1030 wet drum, 1,500 gaussFinal concentrate
Dewatering12 m thickener + disc filter9-10% moisture

The silica problem

Above 67% Fe the limiting impurity in magnetite concentrate is usually silica as finely locked quartz. Adding a reverse flotation stage with an amine collector removes it and can push the concentrate above 69% Fe, which is where direct reduction grade starts. It costs about USD 1.50 per tonne of concentrate and is worth it when the product goes to DR-grade pellets rather than sinter.

Questions we are asked before quoting

Can I use a dry magnetic separator?

Only for coarse cobbling above 5 mm. Below that, dry separation loses selectivity to dust and particle entrainment; wet drums are the only practical option.

What grind do I need?

It depends on the liberation size, which needs a study on your ore. Typical banded magnetite liberates at 45-75 microns; disseminated magnetite in a volcanic host often needs 25-30 microns.

Other solution categories

Same engineering team, different process route.

Send your material. We will send the flow sheet.

Feed size, moisture, target capacity and product spec are enough to start. Quotations and plant layouts are free and usually back within one working day.

Request a flow sheet WhatsApp us