Manganese Ore Magnetic Separation Line

Reviewed 2026-11-27 Bellian Process Engineering

Manganese upgrading by gravity and high-intensity magnetic separation, lifting a 20-30% Mn feed to 38-45% concentrate for ferroalloy and battery use.

Manganese Ore Magnetic Separation Line

Manganese is sold on grade, and the grade breaks fall at very specific points. Below 30% Mn the ore goes to cement or as a blending ore at a discount. Above 38% it goes to silicomanganese furnaces at a real price. Above 44% with low phosphorus it can enter the battery market at several times that. Most manganese beneficiation projects exist to move ore across one of those lines.

Capacity100-800 t/d
Feed grade18-32% Mn
Concentrate38-48% Mn
Recovery70-85%

Oxide and carbonate are different ores

Manganese oxide ore (pyrolusite, psilomelane) is magnetic enough for high-intensity separation and heavy enough for gravity. Manganese carbonate (rhodochrosite) is weakly magnetic and soft, and it slimes badly during grinding — which means the separation has to happen at a coarser size than you would like. The flowsheet has to be chosen on the mineralogy, not on the element.

Ore typeMain mineralRoute
Oxide, coarsePyrolusiteJig + high-intensity magnetic
Oxide, finePsilomelane, wadHigh-gradient magnetic or flotation
CarbonateRhodochrositeHeavy media + magnetic, coarse grind
Mixed with ironFerruginous Mn oreReduction roast then magnetic

Process flow

Crushing to 25 mmWashingJig (2-25 mm)GrindingHigh-intensity magneticDewatering

Washing first

Most manganese ore arrives with 15-30% clay. A drum scrubber and a washing screen remove it before any separation, and that alone lifts the grade by 3-6 points. Skipping the wash stage is the most common reason a manganese plant underperforms.

Gravity on the coarse fraction

A jig on the 2-25 mm fraction separates manganese (specific gravity 4.7-5.0) from quartz and clay (2.6) with good efficiency, rejecting 25-40% of the mass. It is cheap, needs no reagents, and handles the size range that magnetic separators handle badly.

Magnetic on the fine fraction

The minus 2 mm fraction is ground to 80% passing 0.5 mm and passed through a high-intensity magnetic separator at 1.2-1.6 T. Wet high-gradient with a pulsating matrix is preferred because manganese fines blind a static matrix quickly.

Equipment list

StageEquipmentSpecification
CrushingPE-400x600 jaw + roller crusherTo 25 mm
WashingDrum scrubber 1.2 x 3.0 m + washing screenRemove 15-30% clay
GravityJig 2-25 mm, 2 chambersReject 25-40%
GrindingRod mill 1,200 x 3,00080% passing 0.5 mm
MagneticSLon-1000 vertical ring, 1.4 TPulsating matrix
DewateringThickener + filter press10% moisture

Phosphorus, the hidden specification

Most manganese ores carry phosphorus, and steelmakers penalise it hard: each 0.01% P above 0.1% cuts the ore value noticeably. Phosphorus sits in apatite or in the manganese lattice itself. If it is in apatite, a flotation stage with a fatty acid collector removes it. If it is in the lattice, no physical separation will help and the ore is destined for the blending market.

Questions we are asked before quoting

Can I get battery-grade manganese?

Not by physical separation. Battery grade needs 99.5% MnSO4, which means a hydrometallurgical route: leach, purify, crystallise. Physical beneficiation can produce the 44% concentrate that feeds that plant.

What recovery is realistic?

70-85% depending on liberation. Below 70% usually means the manganese is finely disseminated in the gangue and the grind is not fine enough, or the ore contains significant wad that slimes.

Other solution categories

Same engineering team, different process route.

Send your material. We will send the flow sheet.

Feed size, moisture, target capacity and product spec are enough to start. Quotations and plant layouts are free and usually back within one working day.

Request a flow sheet WhatsApp us