Bottom ash is 20-25% of municipal waste by mass and carries 2-5% ferrous and 1-2% aluminium. Ageing, crushing, screening and eddy current separation into a saleable aggregate.

MSW Incinerator Bottom Ash Processing Line

Every tonne of municipal waste burned produces 200-250 kg of bottom ash, and that ash contains about 2-5% ferrous metal, 1-2% aluminium, and a mineral fraction that behaves much like a low-grade sand and gravel. In Europe the ash is regulated as waste but the recovered metals are not, and the mineral fraction after treatment is a recognised construction material in several countries. The plant is a metal recovery plant that happens to produce aggregate.

Capacity100-600 t/d
Ferrous recovery> 90%
Aluminium recovery> 70%
Product moisture< 12%

Why ageing comes first

StepDurationWhat it does
Quench and stockpile6-12 weeksHydrates free lime, oxidises aluminium, cools the ash
CrushingMinutesLiberates metal from the sintered matrix
ScreeningMinutesSeparates 0-4 mm from 4-40 mm
Magnetic separationMinutesRecovers iron and stainless
Eddy currentMinutesRecovers aluminium and copper

Fresh bottom ash contains metallic aluminium that reacts with water to produce hydrogen, and free lime that expands. Aged ash is stable and, critically, its aluminium has oxidised into a non-magnetic state that separates cleanly in an eddy current field. Skipping the ageing step cuts aluminium recovery by half and produces a hydrogen hazard in the storage silo.

Process flow

Quench pitAgeing bayHopperJaw crusherScreenOverbelt magnetEddy currentWashingAggregate stockpile

Crushing and screening

A jaw crusher reduces the ash to below 40 mm; a hammer mill can be used but produces a flatter particle shape and more fines. Screening at 4 mm and 40 mm creates three streams: the fine fraction goes to washing for glass and dense media, the mid fraction to metal recovery, and the oversize returns to the crusher or to landfill.

Metal recovery

An overbelt magnet at 80 mm and a drum magnet at 20 mm recover 88-93% of the ferrous, which sells as a lower-grade scrap because it carries ash and stainless contamination. An eddy current separator on the 4-20 mm fraction recovers aluminium at 70-80% and also picks up copper, brass and lead. The non-ferrous concentrate at 60-75% metal sells to a secondary smelter.

Washing and the aggregate product

Washing removes soluble salts — chlorides and sulphates — that would otherwise leach from the product in service. A attrition scrubber plus a spiral washer brings the chloride content below 0.1%, which is the threshold most specifications set for use as a road base or concrete block aggregate. Without washing, the material is only suitable for landfill capping.

Equipment list

StageEquipmentSpecification
FeedingPlate feeder300 t/d
CrushingJaw crusherTo 40 mm
ScreeningTrommel screen0-4, 4-20, 20-40 mm
FerrousOverbelt + drum magnet1,200 gauss
Non-ferrousEddy current separatorEccentric rotor, 3,000 rpm
WashingAttrition scrubber + spiral washerChloride below 0.1%
Water treatmentClarifier + filter pressClosed loop
Dust and odourBag filter, biofilterOdour control

The product standards that decide the design

If the aggregate is going to a road authority, the specification will set limits on loss on ignition (below 5%), chloride, sulphate, and heavy metals leaching by a standard test. Those limits determine how much washing and how much ageing the plant needs, and they should be read before the flowsheet is drawn rather than after. A plant sized for landfill capping cannot be upgraded to road base later without adding a washing section, which needs water treatment and space that the site plan usually does not have.

Questions we are asked before quoting

How much metal is really in bottom ash?

2-5% ferrous and 1-2% non-ferrous in a typical European or Asian municipal waste stream. In a waste stream with high packaging content the aluminium can reach 2.5%.

Can the ash go to a cement kiln?

The fine fraction can, as a raw meal component, if the chloride is below 0.5%. Above that it causes a kiln bypass requirement.

Other solution categories

Same engineering team, different process route.

Send your material. We will send the flow sheet.

Feed size, moisture, target capacity and product spec are enough to start. Quotations and plant layouts are free and usually back within one working day.

Request a flow sheet WhatsApp us