Henan Bellian Mining Machinery
Home/ Solutions/ Mineral Processing/ Process route
Mineral Processing · Process route

Fluorite Beneficiation Line

Reviewed 2026-11-27 Bellian Process Engineering

Fluorite grades: metallurgical at 70% CaF2, ceramic at 97%, acidspar at 97.5% with silica below 1%. The flotation circuit and the depression chemistry that reaches acidspar.

Fluorite Beneficiation Line

Fluorspar is sold in three grades that differ by a factor of three in price, and the difference between them is a single flotation flowsheet. Metallurgical grade at 70-85% CaF2 goes to steelmaking as a flux and needs only hand sorting and crushing. Acidspar at 97.5% CaF2 with silica below 1% and calcium carbonate below 1.2% goes to hydrofluoric acid and is a flotation product. The jump from one to the other is where the engineering is.

Capacity100-800 t/d
Acidspar97.5% CaF2
SiO2Below 1%
Recovery80-90%

The three grades and their limits

GradeCaF2Key limitUse
Metallurgical70-85%Silica not criticalSteel flux, cement
Ceramic95-97%Fe2O3 below 0.12%Enamel, glass, welding
Acidspar97.5% minSiO2 below 1%, CaCO3 below 1.2%HF, aluminium fluoride

Acidspar is the grade that pays, and the two impurities that block it are quartz and calcite — which float in opposite directions and need different chemistry.

Process flow

Run-of-mineCrushingHand sortingGrindingRougher flotationCleanersMagnetic separationDewateringDrying

Sorting and grinding

Coarse fluorite is often visibly distinct, and hand or optical sorting removes 15-30% of the feed as a metallurgical product before any grinding. That reduces the flotation feed and improves the economics more than any reagent change. Grinding to 80% passing 150-200 micron liberates the fluorite from quartz and calcite; over-grinding below 75 micron creates slime that is hard to float and hard to filter.

Flotation chemistry

Fluorite is floated with a fatty acid collector — oleic acid or tall oil — at pH 9-10, activated by sodium silicate as a quartz depressant. The complication is calcite, which also responds to fatty acids. Two strategies work: depress the calcite with quebracho or tannin at pH 8-9, or float the calcite first with a shorter-chain collector and then float the fluorite. Which one is right depends on the calcite-to-quartz ratio in the ore, and it can only be settled by bench testing.

Heating, the old trick

A conditioning step at 60-85 C with sodium silicate for 30-60 minutes improves the selectivity dramatically by desorbing the collector from the gangue surfaces. It costs energy but lifts the grade by 3-6 points in a single stage, which is why almost every acidspar plant has a heated conditioner.

Iron removal

For ceramic grade the iron limit is 0.12% Fe2O3, which flotation cannot guarantee. A wet high-intensity magnetic separator at 12,000-15,000 gauss after the cleaners removes the iron-bearing minerals, and in some cases the product is leached with dilute acid to reach the specification.

Equipment list

StageEquipmentSpecification
PrimaryJaw crusherTo 60 mm
SortingHand or opticalMetallurgical product out
GrindingBall Mill + classifier80% below 150 micron
ConditioningHeated tank, 80 CSodium silicate, 45 minutes
FlotationRougher + 4 cleanerspH 9-10, fatty acid
MagneticWHIMS, 15,000 gaussIron removal
DewateringThickener + filter + dryerBelow 1% moisture

Tailings and fluoride

Fluoride in the tailings water is a regulated discharge parameter, usually limited to 10-20 mg/L. Lime precipitation plus alum brings it into range and is a standard part of the water circuit. A fluorite plant that ignores this will be shut down in its first year in most jurisdictions, so the water treatment belongs in the flowsheet, not in the environmental annex.

Questions we are asked before quoting

Can I make acidspar from a 40% ore?

Yes, with a five-stage cleaner circuit and a heated conditioner, at 80-85% recovery. The limit is usually the calcite, not the grade of the ore body.

What grind size is best?

Coarse enough to liberate and fine enough to clean. Most ores liberate at 150-200 micron; grinding to 75 micron costs 40% more energy and produces a product that filters badly.

Other solution categories

Same engineering team, different process route.

Send your material. We will send the flow sheet.

Feed size, moisture, target capacity and product spec are enough to start. Quotations and plant layouts are free and usually back within one working day.

Request a flow sheet WhatsApp us