Henan Bellian Mining Machinery
Home/ Solutions/ Cement & Lime/ Process route
Cement & Lime · Process route

LECA Lightweight Aggregate Production Line

Reviewed 2026-11-27 Bellian Process Engineering

Expanded clay aggregate: the raw clay's bloating behaviour decides everything. Kiln profile, the 1,150-1,250 C expansion window, and the bulk density grades the market actually buys.

LECA Lightweight Aggregate Production Line

Lightweight aggregate is made by trapping gas inside a semi-molten pellet. Clay or shale is heated to the point where its surface becomes viscous enough to seal, while inside the pellet a gas is released that cannot escape. The pellet expands three to five times its volume and the gas stays locked in the cooled shell. Whether that happens depends on the clay's composition far more than on the kiln.

Capacity50-300 m3/d
Expansion1,150-1,250 C
Bulk density250-600 kg/m3
Water absorption8-20%

What makes a clay bloating

Three conditions have to coincide inside the pellet, and all three come from the raw material.

ConditionMechanismRaw material requirement
Gas releaseFe2O3 reduction, organic combustion, carbonate decomposition2-8% Fe2O3, 0.5-2% organic carbon
Viscous shellSilica-alumina melt seals the surfaceSiO2 50-65%, Al2O3 12-22%, flux 6-12%
Right temperatureMelt viscosity in the window between sealing and collapseSoftening 1,100 C, collapse above 1,280 C

A clay with 1% iron and no carbon will not expand at any temperature. A clay with 12% iron will expand so violently it shatters. Before building a plant, run a laboratory bloating test on the actual material — this is a two-week test that saves a two-million-dollar mistake.

Process flow

Clay pitStockpileCrushingMixingPelletisingDryerRotary kilnCoolerScreening

Preparation and pelletising

Clay is crushed to below 2 mm, blended with a small amount of fuel or flux if the analysis requires it, and formed into 5-20 mm pellets on a disc or drum pelletiser with 18-25% water. Pellet size uniformity controls the product grading, and grading is what the customer buys: a batch that is half 8 mm and half 16 mm sells at a discount to a screened product.

Drying

Green pellets at 20% moisture cannot go into a kiln at 1,200 C; they explode into fragments. A rotary dryer at 200-300 C brings them down to 3-5% moisture over 25-40 minutes. This is the step that most small plants try to skip with a longer kiln preheat zone, and it is the step that limits their output.

Expansion in the kiln

A rotary kiln with an internal chain or cross section in the preheat zone and a 6-8 minute residence in the 1,150-1,250 C expansion zone. Control is delicate: the kiln is run with a slight reducing atmosphere in the expansion zone to keep the iron in the ferrous state, which is what generates the gas. Too much air and the pellet oxidises and stops expanding; too little and the kiln reduces the shell and the pellets stick into a ring.

Cooling

Rapid cooling in a rotary cooler to below 200 C fixes the structure. Slow cooling allows the melt to crystallise and the pellet loses up to 30% of its expansion.

Equipment list

StageEquipmentSpecification
CrushingRoll crusher + mixerTo 2 mm, blended
PelletisingDisc pelletiser, 3.2 m15 t/h green pellets
DryingRotary dryer 2.2 x 18 m20% to 4% moisture
ExpansionRotary kiln 2.8 x 45 m120 m3/d, 1,200 C
CoolingRotary coolerFast cool to 180 C
ScreeningVibrating screen, 3 decks0-4, 4-8, 8-16 mm
Dust collectionBag filterKiln and cooler

The market grades and what they cost to make

Structural LECA at 400-600 kg/m3 bulk density sells to precast and block plants and is the volume product. Insulation-grade at 250-350 kg/m3 goes into lightweight screeds and geotechnical fill and carries a premium, but the yield is lower because it needs a higher expansion ratio. The kiln produces a spread of densities in every run; the skill is in the screening and in selling the whole spread rather than only the best fraction.

Questions we are asked before quoting

Can I use shale instead of clay?

Yes. Shale is harder to pelletise as it needs finer grinding and more water, but it often has the carbon content that clay lacks.

Can the kiln burn waste oil or biomass?

Usually yes for the preheat and drying zones. The expansion zone needs stable temperature within 20 C, which is easier with a consistent fuel.

Other solution categories

Same engineering team, different process route.

Send your material. We will send the flow sheet.

Feed size, moisture, target capacity and product spec are enough to start. Quotations and plant layouts are free and usually back within one working day.