Polymetallic Tailings Reprocessing

Reviewed 2026-11-27 Bellian Process Engineering

Recovering copper, lead, zinc, gold and magnetite from old tailings with a regrind and flotation circuit, often at a lower cost than mining fresh ore.

Polymetallic Tailings Reprocessing

Old tailings dams are often the cheapest orebody a mine has. They are already broken, already at surface and already permitted. The grade is lower than the original feed but the metallurgy is often easier, because the minerals that were hard to float in 1985 are still there and the technology that could not reach them is now standard.

Capacity200-1,500 t/d
FeedOld tailings, 20-40% solids
ProductsCu / Pb / Zn / Au concentrates
Recovery50-80% of residual metal

What is actually in a tailings dam

A tailings dam is a size-sorted deposit. The coarse sand settled near the discharge point, the slimes travelled further. That means the metal distribution is not uniform, and the first task is a drilling programme to map grade against location and depth. A dam that averages 0.15% Cu can easily contain zones at 0.35% and zones at 0.05%.

The other issue is oxidation. Sulphides at surface oxidise over decades, and oxidised tailings float poorly. The sulphide sulphur content, not the total metal, is what tells you whether flotation will work.

ConditionEffect on recovery
Sulphide sulphur above 1%Flotation viable at 70-85% recovery
Sulphide sulphur 0.3-1%Marginal, needs sulphidisation or bulk float
Heavily oxidised, below 0.3%Leach or gravity only
Slimes above 40% passing 20 micronNeeds desliming before flotation

Process flow

Hydraulic miningSlurry pumpingDeslimingRegrindRougher flotationCleanerThickeningFiltration

Reclaiming

Hydraulic monitors at 8-10 bar break the dam face into a slurry at 25-35% solids, which is pumped to the plant. The alternative — dry excavation and trucking — costs three to five times more per tonne and is only used where the dam cannot be re-slurried.

Desliming and regrinding

Tailings contain far more slime than fresh ore, and slime consumes collector and ruins flotation selectivity. A cyclone desliming stage at 15-20 microns removes it. The sand fraction is then reground, usually lightly, to re-liberate locked particles that the original grind left behind.

Flotation

Essentially the same circuit as the original plant, but at a lower grade and with more reagent. A bulk rougher is often better than selective flotation on tailings, because the residual metal is finely distributed and a bulk concentrate can be sold or further treated.

Equipment list

StageEquipmentNote
Reclaim2 hydraulic monitors + slurry pump25-35% solids
DeslimingCyclone cluster at 18 micronRemoves 30-50% slime
RegrindBall Mill 1,500 x 3,000Light regrind to 100 micron
FlotationRougher 6 + scavenger 4 + cleaner 3Bulk or selective
DewateringThickener + filter pressConcentrate for sale
WaterReturn water pond70-80% recycle

Why the economics often work

There is no drilling, no blasting, no crushing and no primary grinding — four of the five biggest cost centres in a concentrator are already done. Operating cost typically lands at 40-55% of a greenfield plant treating the same tonnage. Against that, the grade is lower and the recovery is lower, so the project works on a specific combination of residual grade and metal price that a feasibility study has to test honestly.

Questions we are asked before quoting

Do I need a new tailings dam?

You need somewhere to put the new tailings. In many cases the reprocessed tailings can be stacked back into the worked-out section of the same dam, which is both cheaper and better for closure.

How long does it take to evaluate a dam?

Three to five months: a drilling and sampling programme, a mineralogical study, and locked-cycle flotation tests. Doing this before committing capital is what separates a viable project from an expensive lesson.

Other solution categories

Same engineering team, different process route.

Send your material. We will send the flow sheet.

Feed size, moisture, target capacity and product spec are enough to start. Quotations and plant layouts are free and usually back within one working day.

Request a flow sheet WhatsApp us