Chromite Beneficiation Line

Reviewed 2026-11-27 Bellian Process Engineering

Chromite is dense, weakly magnetic, and sold on the chromium-to-iron ratio. Gravity concentration, magnetic polishing and the grind size that keeps the ratio above 2.5.

Chromite Beneficiation Line

Chromite is one of the few ores where gravity concentration still does the whole job. At a specific gravity of 4.1-4.9 against a gangue of 2.6-3.0, the density difference is large enough that spirals and shaking tables can produce a marketable concentrate without flotation or chemical reagents. The difficulty is not separation; it is the chromium-to-iron ratio, which is set by the ore body and can only be improved marginally by processing.

Capacity100-1,000 t/d
Cr2O340-48% concentrate
Cr/Fe ratio1.5-3.0
Recovery75-88%

What the three markets demand

MarketCr2O3Cr/FeSize
Metallurgical (ferrochrome)40-44%Above 2.510-80 mm lump, or fines
Chemical (dichromate)44-46%Above 2.0Below 200 mesh
Refractory30-40%Above 1.8Sized, low silica

The ratio matters because ferrochrome smelting is a reduction of chromium with carbon, and iron reduces first and takes the carbon with it. A charge with a Cr/Fe of 1.8 cannot produce high-carbon ferrochrome above 60% Cr at any reasonable energy input. This is a deposit property, not a plant property — verify it before designing anything.

Process flow

Run-of-mineJaw crusherScreenRod millSpiral concentratorShaking tableMagnetic separatorDewatering

Crushing and grinding

Chromite liberation is coarse — 80% liberation at 1-3 mm for most stratiform ores — which is why rod mills are preferred over Ball Mills: they produce less slime, and slime is the enemy of gravity separation. Grinding to 1 mm liberates most of the chromite at less than half the energy of grinding to 75 micron. A ball mill is used only for the fine chemical-grade product.

Gravity concentration

Rougher spirals at 1-3 mm produce a 35-42% Cr2O3 concentrate at 80-85% recovery. A cleaner spiral and a shaking table on the rougher concentrate lift the grade to 44-48% with a combined recovery of 75-88%. The spiral circuit needs a stable pulp density at 25-35% solids; fluctuations of 10% in density cost 5 points of recovery, which is why a proper distributor and density control matter more than the number of spiral starts.

Magnetic polishing

Chromite is weakly magnetic and the iron-bearing gangue — serpentine with magnetite, and occasionally chromite with high iron — responds differently. A high-intensity magnetic separator at 10,000-15,000 gauss on the gravity concentrate removes the iron-rich fraction and lifts the Cr/Fe ratio by 0.2-0.5. For refractory-grade product, a low-intensity pass removes free magnetite first.

Equipment list

StageEquipmentSpecification
PrimaryJaw crusherTo 50 mm
SecondaryCone crusherTo 5 mm
GrindingRod mill 1.8 x 3.6 mTo 1 mm, low slime
RougherSpiral concentrator, 2 stages25-35% solids
CleanerShaking tableConcentrate 46% Cr2O3
MagneticHigh intensity, 15,000 gaussLifts Cr/Fe
DewateringThickener + filterBelow 10% moisture

The slime problem

Fines below 75 micron are the main loss in a chromite plant, and in a poorly operated circuit they can carry 15-25% of the chromium to tailings. Two fixes: grind coarser, and treat the slimes separately with a fine spiral, a Falcon or a Kelsey jig. A slime circuit costs 15% of the plant capital and typically recovers 8-12% more chromium, which usually pays for itself within two years.

Questions we are asked before quoting

Is flotation ever used for chromite?

Rarely. It is used for very fine intergrowths and for reducing silica in chemical-grade concentrate, but gravity is cheaper and the density difference is large enough that flotation is only justified when gravity cannot meet the silica specification.

What is the minimum viable tonnage?

Around 100 t/d for a gravity-only plant with a table cleaner. Below that the labour and assaying costs dominate.

Other solution categories

Same engineering team, different process route.

Send your material. We will send the flow sheet.

Feed size, moisture, target capacity and product spec are enough to start. Quotations and plant layouts are free and usually back within one working day.

Request a flow sheet WhatsApp us