Dolomite Calcination Line
Dolomite decomposes in two steps, which is why it cannot be calcined like limestone. The temperature window, the kiln choice for caustic and dead-burned grades, and the hydration risk in storage.

Dolomite is not limestone with magnesium in it. CaMg(CO3)2 decomposes in two separate steps: magnesium carbonate breaks down at 700-750 C and calcium carbonate at 880-920 C. A kiln that heats uniformly through both windows produces a sound product; a kiln that overshoots the first step before the second begins produces a material with uneven reactivity that fails the customer's test. This two-step behaviour governs the whole plant design.
Three products, three temperature regimes
| Product | Temperature | Bulk density | Use |
|---|---|---|---|
| Caustic calcined dolomite | 800-1,000 C | 1.0-1.4 g/cm3 | Magnesium source, water treatment, soil |
| Sintered dolomite | 1,600-1,700 C | 2.8-3.0 g/cm3 | Refractory bricks, gunning mixes |
| Dead burned dolomite | 1,700-1,800 C | 3.0-3.2 g/cm3 | Steel ladle lining, fettling |
The step from caustic to dead burned is a different plant, not a different setting. Dead burning needs a rotary kiln with a sintering zone, high-alumina or basic refractory, and a cooler that can handle 1,800 C clinker. A shaft kiln cannot reach it.
Process flow
Feed sizing
A vertical shaft kiln needs 40-80 mm lump with less than 10% fines, screened before charging. A rotary kiln accepts 10-40 mm. In both cases the size band matters more than the average: a kiln fed a 20-100 mm spread will over-burn the fines and under-burn the lumps, and the product's reactivity will vary by a factor of two from one truck to the next. Screening is the cheapest quality control in the plant.
Calcination
For caustic grade a rotary kiln at 900-1,050 C with 2-3 hours residence, or a vertical shaft kiln at 70-90 kg of coal per tonne. The shaft kiln is 20-30% more fuel efficient and produces a denser, less reactive product; the rotary kiln gives a more uniform and more reactive product but burns 110-140 kg per tonne. Which one is right depends on whether the customer is buying reactivity or buying density.
Cooling and the hydration problem
Caustic calcined dolomite is hygroscopic and, unlike quicklime, it does not slake violently — it crumbles slowly over weeks. The practical consequence is that the product must be cooled below 80 C and stored dry. A stockpile left in humid air loses 1-2% of its available MgO per month. Indirect cooling and a covered shed are not luxuries in a wet climate.
Equipment list
| Stage | Equipment | Specification |
|---|---|---|
| Crushing | Jaw crusher + roll crusher | To 40 mm |
| Screening | Vibrating screen | 40-80 mm kiln feed |
| Kiln | Rotary kiln 2.8 x 60 m | 250 t/d at 1,000 C |
| Cooler | Rotary or grate cooler | To 80 C |
| Grinding | Raymond Mill, optional | 200 mesh for agricultural grade |
| Collection | Bag filter | 20 mg/m3 |
| Storage | Covered silo or shed | Sealed against humidity |
What to test before committing to a deposit
Not all dolomite dead-burns to a refractory-grade product. The ratio of CaO to MgO should be close to 1:1, silica and alumina should be below 1.5% combined, and the iron content should be below 0.5% for white grades. Crystal size in the raw stone also matters: a finely crystalline dolomite will not grow the 60-100 micron periclase crystals that give a dead-burned product its hydration resistance, no matter what the kiln does.
Questions we are asked before quoting
Can the same kiln make caustic and dead burned dolomite?
Not well. Dead burning needs 1,750 C and basic refractory; the same kiln at 950 C will run but the refractory will not tolerate the campaign change. Two kilns, or one kiln and a specialist supplier.
How do I stop the product from falling apart in storage?
Cool it below 80 C, keep it dry, and if it is dead burned, check the hydration resistance with an autoclave test rather than trusting the bulk density alone.
Other solution categories