Henan Bellian Mining Machinery
Waste & Slag Recycling · Process route

Silicomanganese and Ferroalloy Slag Processing

Reviewed 2026-11-27 Bellian Process Engineering

Ferroalloy slag carries 8-20% entrained metal and a manganese content that is both a resource and an environmental limit. Recovery, drying and the cement route.

Silicomanganese and Ferroalloy Slag Processing

Ferroalloy furnaces produce slag at 1.0-1.4 tonnes per tonne of alloy, and that slag leaves the furnace at 1,600 C carrying entrained metal droplets and 8-20% manganese as oxide. Two problems, one plant: recover the metal because it is worth money, and stabilise or use the residue because manganese leaching is regulated in most jurisdictions and a slag heap that leaches is a liability.

Capacity100-600 t/d
Metal recovery> 80%
Mn in slag8-20%
Product moisture< 1%

Two slag types, two behaviours

SlagCoolingCharacterRoute
Silicomanganese, granulatedWater quenchGlassy, friable, 0-5 mmDewater, dry, magnet, grind
Silicomanganese, lumpAir cooledHard, crystalline, up to 300 mmCrush, screen, magnet
FerrochromeAir cooledVery hard, 5-12% CrCrush, magnet, dry
FerrosiliconAir cooledFriable, low metalCrush, screen, sell

Granulated slag is the easier feed because it is already fine, but it arrives at 15-25% moisture and cannot be magnetically separated wet without losing efficiency. Drying comes first in that route.

Process flow

Slag bayDewateringDryerCrushingScreenMagnetic separationMetal productSlag product

Metal recovery

Entrained alloy is recovered by crushing to below 10 mm and magnetic separation — ferrosilicon and silicomanganese are both magnetic enough for a drum separator at 1,000-1,500 gauss. Recovery reaches 80-88% of the entrained metal, and the recovered product at 60-75% Mn returns to the furnace. Every percentage point of manganese recovered is worth more than the entire processing cost of the tonne it came from.

Drying

Wet granulated slag at 20% moisture is dried in a rotary dryer at 400-500 C inlet gas. Manganese slag dust is fine and abrasive; the dryer needs a cyclone and a bag filter in series, and the bag filter bags should be antistatic because the dry dust is prone to static buildup in pneumatic conveying.

The residue route

After metal recovery the slag still contains 6-12% MnO and is a usable cement kiln feed or a pozzolanic addition. As a cement raw meal component it substitutes for iron and manganese correction, which most plants buy separately. As a supplementary cementitious material, granulated manganese slag gives 70-80% of the strength activity of GGBS at the same fineness. What it must not be is an open heap: manganese at 6% leaches at 2-8 mg/L in an acidic rain environment and exceeds most discharge limits.

Equipment list

StageEquipmentSpecification
DewateringDewatering screenFrom 20% to 12% moisture
DryingRotary dryer 1.8 x 14 mTo below 1%
CrushingJaw + roll crusherTo 10 mm
ScreeningVibrating screen, 2 decks0-3, 3-10 mm
Magnetic separationDrum separator, 1,500 gaussTwo passes
Dust controlCyclone + bag filter10 mg/m3
Product handlingBulk bags or tipperMetal and slag separately

Why ferronickel and ferrochrome are harder

Ferrochrome slag is the most abrasive material in this family at Mohs 7-8 with a chromium spinel phase, and its dust is a hexavalent chromium risk if the slag is exposed to high temperature and alkaline conditions. Handling it needs enclosed conveying, water sprays and personal protection that most slag yards do not have. Ferronickel slag behaves like a low-grade stainless slag and is usually sold as a construction sand after metal recovery.

Questions we are asked before quoting

Can I recover metal from old slag heaps?

Yes, and it is often the best first project: the metal has already been liberated by weathering and the recovery per tonne can exceed fresh slag. Sample the heap at depth first — the top layer is usually oxidised.

What moisture can the dryer take?

Up to 25% for granulated slag, at the cost of a longer drum and more fuel. Above 25% a dewatering screen ahead of the dryer pays for itself.

Other solution categories

Same engineering team, different process route.

Send your material. We will send the flow sheet.

Feed size, moisture, target capacity and product spec are enough to start. Quotations and plant layouts are free and usually back within one working day.

Request a flow sheet WhatsApp us